I-FVL-7435 Liquid Fluorosilicone

I-FVL-7435 Liquid Fluorosilicone Rubber inokumelana okuhle kakhulu namazinga okushisa aphezulu naphansi, ukumelana nowoyela kanye nokufakwa kukagesi, futhi ingelapheka ekamelweni lokushisa.
  • I-FVL-7435

  • I-Herchy

Ukutholakala:
Ubuningi:

Ukusebenza Komkhiqizo

Izinto

Izindlela Zokuhlola

I-NFS-L-7435

Ukubukeka A

ukuhlola okubonwayo

phuzi

Ukubukeka B

ukuhlola okubonwayo

phuzi

Viscosity / Pa.s A

(izinga lokugunda amasekhondi ayi-10 -1 )

Q/371002WXH028-2016

350

Viscosity / Pa.s B

(izinga lokugunda amasekhondi ayi-10 -1 )

Q/371002WXH028-2016

300

25℃×48h

Amandla Adonsela phansi Athize/g/cm3

I-ASTM D792

1.42

Ukuqina/UguA

I-ASTM D2240

35

Amandla Okuqina/MPa

I-ASTM D412

8.1

Ukwelula Ngekhefu /%

I-ASTM D412

320

Amandla Ezinyembezi/KN/m

I-ASTM D624-B

14.5

Ukuqina/%

I-ASTM D1054

36

I-Compression Set/% (177℃×22h)

I-ASTM D395

21

I-Fuel C

Ukushintsha Kwevolumu /%

(25℃×72h)

I-ASTM D471

24.0

Ukusetshenziswa:

I-NFS-L-7435 irabha ye-fluorosilicone ewuketshezi igcwele izingxenye ezimbili. Uma usebenzisa, izingxenye ze-A, B ngokuhambisana nenani lesilinganiso se-1: 1 sokuxuba nokukhipha amagwebu, izinga lokushisa legumbi (25 ℃ ± 5 ℃) elibekwe ku-48h lingelapheka ngokuphelele.

Ukupakisha:

Ipakishwe ngesigubhu sepulasitiki, 20kg engxenyeni ngayinye ye-A/B.

Isikhathi sokugcina:

Igcinwe endaweni epholile neyomile, isikhathi esingavulwa sokugcina sokupakisha esiyizinyanga eziyishumi nambili.

Izinyathelo zokuzivikela:

Gwema ukuthintana nezinhlanganisela eziqukethe i-nitrogen, isulfure, i-phosphorus nezinsimbi ezisindayo, ezingase zidale ukuthi umkhiqizo uqhume ungaphekiwe noma ungavuthi.

Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.