FVL-7435 Fluorosilicone dareere ah

FVL-7435 Liquid Fluorosilicone Rubber waxay leedahay iska caabin heer sare ah iyo heerkul hoose, caabbinta saliidda iyo dahaarka korantada, waxaana lagu daweyn karaa heerkulka qolka.
  • FVL-7435

  • Herchy

Helitaanka:
Tirada:

Waxqabadka Alaabta

Walxaha

Hababka Imtixaanka

NFS-L-7435

Muuqashada A

qiimeyn muuqaal ah

huruud ah

Muuqashada B

qiimeyn muuqaal ah

huruud ah

Viscosity / Pa.s A

(heerka goynta 10 s -1 )

Q/371002WXH028-2016

350

Viscosity / Pa.s B

(heerka goynta 10 s -1 )

Q/371002WXH028-2016

300

25℃×48h

Cufis-jiidad gaar ah/g/cm3

ASTM D792

1.42

Adag/Ceebta A

ASTM D2240

35

Xoojinta Xoojinta/MPa

ASTM D412

8.1

Kordhinta Waqtiga Nasashada /%

ASTM D412

320

Xoog jeexjeexa/KN/m

ASTM D624-B

14.5

adkeysi/%

ASTM D1054

36

Dejinta cadaadiska/%(177℃×22h)

ASTM D395

21

Shidaalka C

Bedelka codka /%

(25℃×72h)

ASTM D471

24.0

Isticmaalka:

NFS-L-7435 caag fluorosilicone dareere ah ayaa lagu soo guray laba qaybood. Marka la isticmaalayo, qaybaha A, B sida waafaqsan saamiga mass ee 1: 1 qaso iyo daawaynta defoaming, heerkulka qolka (25 ℃ ± 5 ℃) meeleeyay 48h si buuxda loo dawayn karaa.

Baakad:

Ku jira durbaan caag ah, 20kg qayb kasta oo A/B ah.

Xilliga kaydinta:

Lagu kaydiyaa meel qabow oo qalalan, oo aan furnayn wakhtiga kaydinta baakadaha asalka ah oo laba iyo toban bilood ah.

Ka taxadaritaan:

Iska ilaali inaad la xiriirto xeryahooda ay ku jiraan nitrogen, sulfur, fosfooraska iyo biraha culus, kuwaas oo keeni kara in alaabtu ay vulcanize iyada oo aan la karinin ama aysan vulcanise.

Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.