FVL-7435 Fluorosilicone Cairan

FVL-7435 Fluorosilicone Rubber nduweni resistance banget kanggo suhu dhuwur lan kurang, resistance lenga lan jampel electrical, lan bisa nambani ing suhu kamar.
  • FVL-7435

  • Herchy

kasedhiyan:
Jumlah:

Kinerja Produk

barang

Metode Tes

NFS-L-7435

Penampilan A

pambiji visual

kekuningan

Penampilan B

pambiji visual

kekuningan

Viskositas / Pa.s A

(laju geser 10 s -1 )

Q/371002WXH028-2016

350

Viskositas / Pa.s B

(laju geser 10 s -1 )

Q/371002WXH028-2016

300

25 ℃ × 48 jam

Gravitasi spesifik/g/cm3

ASTM D792

1.42

Kekerasan / ShoreA

ASTM D2240

35

Kekuatan Tarik/MPa

ASTM D412

8.1

Elongation ing Break /%

ASTM D412

320

Kekuwatan luh/KN/m

ASTM D624-B

14.5

Ketahanan/%

ASTM D1054

36

Set Kompresi/%(177℃×22j)

ASTM D395

21

Bahan bakar C

Ganti Volume /%

(25℃×72h)

ASTM D471

24.0

Dianggo:

NFS-L-7435 karet fluorosilicone cair dikemas ing rong komponen. Nalika nggunakake, komponen A, B sesuai karo rasio massa 1: 1 nyawiji lan perawatan defoaming, suhu kamar (25 ℃ ± 5 ℃) diselehake ing 48h bisa nambani rampung.

Packing:

Dikempalken ing drum plastik, 20kg kanggo saben komponen A/B.

Periode panyimpenan:

Disimpen ing lingkungan sing adhem lan garing, wektu panyimpenan kemasan asli sing durung dibukak rolas wulan.

Cegahan:

Aja kontak karo senyawa sing ngemot nitrogen, belerang, fosfor lan logam abot, sing bisa nyebabake prodhuk kasebut vulcanise mentah utawa ora vulcanise.

Sadurunge: 
Sabanjure: 

LINKS CEPAT

PRODUK KAMI

INFORMASI KONTAK

Tambah: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telpon / WhatsApp / Skype: +86 15221953351
Hak Cipta     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Kebijakan Privasi | Dhukungan dening Leadong.