FVL-7435 na ɛwɔ hɔ
Herchy a ɔyɛ ɔbarima
| Nea Ɛwɔ Hɔ: | |
|---|---|
| Dodow: | |
Nneɛma |
Akwan a Wɔfa so Sɔ Sɔhwɛ |
NFS-L-7435 na ɛwɔ hɔ |
Sɛnea ɛte A |
aniwa so nhwehwɛmu |
ɛyɛ kɔkɔɔ |
Sɛnea ɛte B |
aniwa so nhwehwɛmu |
ɛyɛ kɔkɔɔ |
Nsuo a ɛyɛ den / Pa.s A (nsu a ɛtwetwe 10 s -1 ) . |
Asɛmmisa/371002WXH028-2016 |
350 |
Nsuo a ɛyɛ den / Pa.s B (nsu a ɛtwetwe 10 s -1 ) . |
Asɛmmisa/371002WXH028-2016 |
300 |
25°C×48h na ɛwɔ hɔ |
||
Nneɛma a ɛtwe ade ba fam pɔtee/g/cm3 |
ASTM D792 na ɛwɔ hɔ |
1.42 |
Nneɛma a ɛyɛ den/MpoanoA |
ASTM D2240 na ɛwɔ hɔ |
35 |
Tensile Ahoɔden/MPa |
ASTM D412 na ɛwɔ hɔ |
8.1 |
Elongation Wɔ Ahomegye Mu /% . |
ASTM D412 na ɛwɔ hɔ |
320 |
Nsuo Ahoɔden/KN/m |
ASTM D624-B na ɛwɔ hɔ |
14.5 |
Nketesie/% |
ASTM D1054 na ɛwɔ hɔ |
36 |
Nhyɛso Set/%(177°C×22h) . |
ASTM D395 na ɛwɔ hɔ |
21 |
Petrol a wɔde yɛ C Volume Nsakrae /% . (25°C×72h) . |
ASTM D471 na ɛwɔ hɔ |
24.0 |
Sɛnea wɔde di dwuma:
Wɔde NFS-L-7435 nsu fluorosilicone rɔba ahyɛ mu wɔ nneɛma abien mu. Sɛ wode, A, B afã horow di dwuma sɛnea mass ratio a ɛyɛ 1:1 afrafra ne defoaming ayaresa, dan mu hyew (25 °C ± 5 °C) a wɔde ahyɛ 48h mu no betumi asa koraa.
Nneɛma a wɔde kyekyere nneɛma:
Wɔde ahyɛ plastic drum mu, 20kg ma A/B fã biara.
Bere a wɔde sie:
Wɔde sie baabi a ɛhɔ yɛ nwini na ɛhɔ yɛ kusuu, a wɔanbue mfitiase nneɛma a wɔde sie no bere a wɔde asie asram dumien.
Ahwɛyiye a ɛsɛ sɛ yɛyɛ:
Kwati sɛ wobɛka nneɛma a nitrogen, sulphur, phosphorus ne dade a emu yɛ duru wom, a ebetumi ama ade no ayɛ vulcanise a wɔnnoa anaasɛ ɛnnyɛ vulcanise.