FV9502
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Items | Index | ||
Serial number | FV9552 | FV9562 | |
Appearance Test Methods | yellowish | ||
Specific Gravity/ g/cm3 | ASTM D792 | 1.42 | 1.43 |
Hardness/shoreA | ASTM D2240 | 52 | 61 |
Tensile Strength/MPa | ASTM D412 | 10.2 | 9.4 |
Elongation At Break /% | ASTM D412 | 330 | 280 |
Tear Strength/KN/m | ASTM D624-B | 20 | 19 |
Compression Set(177℃*22h ) | ASTM D395 | 7 | 8 |
Resilience/% | ASTM D1054 | 35 | 34 |
*Heat Resistance | Hardness change /shore A | 2 | 2 |
Hardness change /shore A | -24 | -23 | |
Elongation at break change, % | -21 | -20 | |
Fuel C | ASTM D471 | 22 | 21 |
Curing Condition | 0.5 parts of bis-2-5, one stage vulcanisation 170℃×15min, two stage vulcanisation: 200℃×4h | ||
Recommended actions:
It's suggested to utilize 0.4-0.7 parts of bisdisulfide (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).
Customers should choose the most appropriate temperature and time for curing based on the product's size and method of curing.
Product packaging:
This product is not dangerous, it's instead composed of cardstock, plastic, and 10 kilograms per bag, 2 bags per box.
Age of storage:
This product has a cold flow capacity, the bag should be avoided in order to not have it damaged during transportation or utilization.
Keep in a cool, dry environment with a shelf life of 12 months.