FVL-7435
Herchy
| Nnweta: | |
|---|---|
| Ọnụọgụ: | |
Ihe |
Ụzọ ule |
NFS-L-7435 |
Mpụta A |
nlele anya |
odo odo |
Ọdịdị B |
nlele anya |
odo odo |
Viscosity / Pa.s A (ọnụego shear 10 s -1 ) |
Q/371002WXH028-2016 |
350 |
Viscosity / Pa.s B (ọnụego shear 10 s -1 ) |
Q/371002WXH028-2016 |
300 |
25 ℃ × 48h |
||
Specific ike ndọda/g/cm3 |
ASTM D792 |
1.42 |
Isi ike/ikpere mmiriA |
ASTM D2240 |
35 |
Ike tensile/MPa |
ASTM D412 |
8.1 |
Nkwalite na ezumike /% |
ASTM D412 |
320 |
Ike akwa/KN/m |
ASTM D624-B |
14.5 |
Nkwụsị ike/% |
ASTM D1054 |
36 |
Ntọala mkpakọ/% (177 ℃ × 22h) |
ASTM D395 |
21 |
Mmanụ ụgbọala C Mgbanwe olu /% (25 ℃ × 72h) |
ASTM D471 |
24.0 |
Ojiji:
NFS-L-7435 roba fluorosilicon mmiri mmiri juru n'ime akụkụ abụọ. Mgbe eji, A, B components dị na uka ruru 1: 1 Ịgwakọta na defoaming ọgwụgwọ, ụlọ okpomọkụ (25 ℃ ± 5 ℃) enịm ke 48h nwere ike gwọọ kpamkpam.
Nkwakọ ngwaahịa:
Ejiri ya na drum rọba, 20kg maka akụrụngwa A/B nke ọ bụla.
Oge nchekwa:
Echekwara ya na ebe dị jụụ ma kpọọ nkụ, oge nchekwa nkwakọ ngwaahịa mbụ na-emegheghị ọnwa iri na abụọ.
Mkpachapụ anya:
Zere kọntaktị na ogige ndị nwere nitrogen, sọlfọ, phosphorus na ọla dị arọ, nke nwere ike ime ka ngwaahịa ahụ pụta ìhè n'esighi ya ma ọ bụ ghara ikpughe.