Muli pano: Kunyumba » Zogulitsa » Synthesis Rubber

Ma Rubber Opangira: Katundu Watsatanetsatane, Ubwino, ndi Ntchito

1. Fluororubber (FKM)

  • Katundu:

    • Kukana kutentha kwambiri (-20 ° C mpaka +250 ° C).

    • Kukana kwapadera kwa mafuta, mafuta, zosungunulira, ma asidi, ndi mabasi.

    • Kulimba kwamphamvu kwambiri, kutsika kwapang'onopang'ono, komanso kukhazikika kwamphamvu kwamankhwala.

    • Kulimbana ndi moto ndi ozoni.

  • Ubwino:

    • Imalimbana ndi mankhwala aukali komanso malo opanikizika kwambiri.

    • Moyo wautali wautumiki muzamlengalenga ndi ntchito zamagalimoto.

  • Mapulogalamu:

    • Zosindikizira zamafuta a ndege, ma O-mphete, ndi ma gaskets.

    • Zisindikizo zotumizira magalimoto, ma hose a injini, ndi zida za turbocharger.

    • Chemical processing zida linings ndi gaskets.

2. Mpira wa Chloroprene (CR)

  • Katundu:

    • Kukana kwamafuta pang'ono (kuposa mphira wachilengedwe koma kuchepera FKM).

    • Cholepheretsa moto chokhala ndi zinthu zozimitsa zokha.

    • Kukana kwanyengo (UV, ozoni, ndi chinyezi).

    • Kusinthasintha pa kutentha kochepa (-40 ° C mpaka + 120 ° C).

  • Ubwino:

    • Zotsika mtengo ndi kukonza kosavuta (extrusion/kuumba).

    • Mkulu makina mphamvu ndi abrasion kukana.

  • Mapulogalamu:

    • Zovala zonyowa, magolovesi, ndi ma hoses a mafakitale.

    • Zomatira za nsapato ndi zomangamanga.

    • Ma jekete achingwe ndi nembanemba zadenga.

3. Mpira wa Nitrile wa Hydrogenated (HNBR)

  • Katundu:

    • Kutentha kwamphamvu (mpaka +150 ° C) poyerekeza ndi NBR.

    • Kukana kwakukulu kwa mafuta, madzimadzi amadzimadzi, ndi amines.

    • Kulimba kwamphamvu kwambiri komanso kukana kutopa.

    • Low permeability kwa mpweya.

  • Ubwino:

    • Imasunga elasticity pansi pa kukhudzidwa kwanthawi yayitali ndi mankhwala owopsa.

    • Kutalika kwa moyo kuposa NBR m'malo ovuta kwambiri.

  • Mapulogalamu:

    • Mafuta ndi gasi pobowola zida (packers, zisindikizo).

    • Malamba oyendera nthawi yamagalimoto, zida za jakisoni wamafuta, ndi zisindikizo za turbocharger.

    • Industrial hydraulic cylinders.

4. Mpira wa Silicone (VMQ)

  • Katundu:

    • Kutentha kwakukulu kwambiri (-60 ° C mpaka +200 ° C).

    • Kuthamanga kwakukulu (mpaka 1000% elongation).

    • Kusungunula kwabwino kwamagetsi komanso kukhazikika kwamafuta.

    • Biocompatible ndi inert.

  • Ubwino:

    • Amasunga kusinthasintha m'malo okhala ndi cryogenic komanso kutentha kwambiri.

    • Kulimbana ndi UV, ozoni, ndi nyengo.

  • Mapulogalamu:

    • Zida zamankhwala (catheters, implants).

    • Zida zamagetsi (ma insulators, keypad).

    • Ma gaskets otentha kwambiri a uvuni ndi injini.

5. Fluorosilicone Rubber (FVMQ)

  • Katundu:

    • Zimaphatikiza kukana kwa mankhwala a FKM ndi kusinthasintha kwa VMQ.

    • Kutentha kwapakati: -50°C mpaka +230°C.

    • Kusamva mafuta, mafuta, ndi madzimadzi amadzimadzi.

    • Kupanikizika kochepa komanso kupirira bwino.

  • Ubwino:

    • Zimagwira pa kutentha kwambiri komanso kutentha kwambiri.

    • Kulimbana ndi kutupa kwamafuta oyendetsa ndege.

  • Mapulogalamu:

    • Zida zamafuta a ndege (mavavu, zisindikizo).

    • Ma gaskets ozama m'nyanja ndi zolumikizira.

    • Masensa agalimoto ndi machitidwe owongolera utsi.

6. Ethylene Propylene Diene Monomer (EPDM)

  • Katundu:

    • Ozone yabwino kwambiri komanso kukana kwanyengo.

    • Mphamvu yapamwamba ya dielectric ndi kukana madzi.

    • Kutentha kwapakati: -50°C mpaka +150°C.

    • Low mpweya permeability.

  • Ubwino:

    • Zotsika mtengo kwambiri pazogwiritsa ntchito panja.

    • Kugwedera kwabwino kwambiri komanso kuchepetsa phokoso.

  • Mapulogalamu:

    • Kuwongolera nyengo yamagalimoto, mapaipi a radiator, ndi zisindikizo zapatsogolo.

    • Zipinda zapadenga ndi dziwe lamadzi.

    • Kutsekereza chingwe chamagetsi ndi malamba otumizira mphamvu.


MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.