GA-2029X
Herchy
| Disponibilitéit: | |
|---|---|
| Quantitéit: | |
Test: 130°C x 5min x 15MPa
| Produit Parameteren | |||||||
| Produit | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | |
| Ausgesinn | Duerchsichteg | ||||||
| Viskositéit (Pa.s) |
A: 1000 B: 2000 |
A: 2000 B: 3000 |
A: 2000 B: 4000 |
A: 2000 B: 4000 |
A: 2000 B: 4000 |
A: 5000 B: 6000 |
|
| Hardness (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Dicht (g/cm3) | 5 | 7 | 8 | 8 | 8 |
7 |
|
| Tensile Stäerkt (MPa) | 900 |
600 |
550 |
500 |
400 |
250 |
|
| Verlängerung (%) | 10 | 10 | 15 | 25 | 25 |
30 |
|
| Tréinekraaft (kN/m) | 16 | 30 | 35 |
40 | 35 |
30 |
|