Caag silikoon dareere ah oo iskii isku dhejiyay (LSR)

Codsiga: isku xidhka substrates balaastikada ah, sida, PC, PA, PET, PBT, PPSU, PEIetc.
Astaamaha muhiimka ah: xoog sare, isku xidhid xoog leh, vulcanization heerkulka hoose.
  • GA-2029X

  • Herchy

Helitaanka:
Tirada:

Tijaabada: 130°C x 5min x 15MPa


Xuduudaha alaabta
Alaabta GA-2029X GA-2029X GA-2029X GA-2029X GA-2029X GA-2029X
Muuqashada Translucent

Viscosity (Pa.s)

A:1000

B:2000

A:2000

B:3000

A:2000

B:4000

A:2000

B:4000

A:2000

B:4000

A:5000

B:6000
Adag ( ShoreA) 20 30 40 50
60
70
Cufnaanta (g/cm3) 5 7 8 8 8
7
Xoog xajin (MPa) 900
600
550
500
400
250
Dheeraynta(%) 10 10 15 25 25
30
Xoogga jeexjeexa (kN/m) 16 30 35
40 35
30










Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.