GA-2029X
Herchy
| kasadiaan: | |
|---|---|
| kuantitas: | |
Uji: 130°C x 5mnt x 15MPa
| Parameter produk | |||||||
| produk | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | |
| Penampilan | Tembus cahaya | ||||||
| Viskositas (Pa.s) |
A: 1000 B: 2000 |
A: 2000 B: 3000 |
A: 2000 B: 4000 |
A: 2000 B: 4000 |
A: 2000 B: 4000 |
A: 5000 B: 6000 |
|
| Teu karasa (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Kapadetan (g/cm3) | 5 | 7 | 8 | 8 | 8 |
7 |
|
| Kakuatan tegangan (MPa) | 900 |
600 |
550 |
500 |
400 |
250 |
|
| Elongation(%) | 10 | 10 | 15 | 25 | 25 |
30 |
|
| Kakuatan cimata (kN/m) | 16 | 30 | 35 |
40 | 35 |
30 |
|