GA-2029X
हेरची
| उपलब्धता: | |
|---|---|
| प्रमाण: | |
चाचणी: 130°C x 5min x 15MPa
| उत्पादन मापदंड | |||||||
| उत्पादन | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | |
| देखावा | पारदर्शक | ||||||
| स्निग्धता (Pa.s) |
A:1000 B:2000 |
A:2000 B:3000 |
A:2000 B:4000 |
A:2000 B:4000 |
A:2000 B:4000 |
A:5000 B:6000 |
|
| कडकपणा (किनारा) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| घनता(g/cm3) | 5 | 7 | 8 | 8 | 8 |
7 |
|
| तन्य शक्ती (MPa) | 900 |
600 |
550 |
500 |
400 |
250 |
|
| वाढवणे(%) | 10 | 10 | 15 | 25 | 25 |
30 |
|
| अश्रू शक्ती (kN/m) | 16 | 30 | 35 |
40 | 35 |
30 |
|