Ucingo: +86 15221953351 I-imeyili: info@herchyrubber.com
Please Choose Your Language
IMIKHIQIZO
Ulapha: Ikhaya » Imikhiqizo » Irabha Yokuhlanganisa » I-Silicone ye-VMQ ) Ukukhetha irabha ye-silicone eyi-self-adhesive (LSR

iyalayisha

Yabelana ku-:
inkinobho yokwabelana ye-facebook
inkinobho yokwabelana ye-twitter
inkinobho yokwabelana ngomugqa
inkinobho yokwabelana ye-wechat
inkinobho yokwabelana ye-linkedin
inkinobho yokwabelana ye-pinterest
inkinobho yokwabelana ye-whatsapp
yabelana ngale nkinobho yokwabela

Irabha ye-silicone eyi-self-adhesive eyi-self-adhesive (LSR)

Isicelo: isibopho nge substrates plastic, ezifana, PC, PA, PET, PBT, PPSU, PEIetc.
Izici eziyinhloko: amandla aphezulu, ukubopha okuqinile, ukushisa okuphansi kwe-vulcanization.
  • I-GA-2029X

  • I-Herchy

Ukutholakala:
Ubuningi:

Isivivinyo: 130°C x 5min x 15MPa


Imingcele yomkhiqizo
Umkhiqizo I-GA-2029X I-GA-2029X I-GA-2029X I-GA-2029X I-GA-2029X I-GA-2029X
Ukubukeka I-Translucent

I-Viscosity(Pa.s)

A:1000

B:2000

A:2000

B:3000

A:2000

B:4000

A:2000

B:4000

A:2000

B:4000

A:5000

B:6000
Ukuqina (ShoreA) 20 30 40 50
60
70
Ukuminyana(g/cm3) 5 7 8 8 8
7
Amandla e-Tensile (MPa) 900
600
550
500
400
250
Ubude(%) 10 10 15 25 25
30
Amandla wezinyembezi (kN/m) 16 30 35
40 35
30










Okwedlule: 
Olandelayo: 

IZIXHUMANISI EZISHESHAYO

IMIKHIQIZO YETHU

ULWAZI LOKUXHUMANA

Engeza: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Ucingo / WhatsApp / Skype: +86 15221953351
I-imeyili:  info@herchyrubber.com
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Imephu yesayithi |   Inqubomgomo Yobumfihlo | Sekela Ngu I-Leadong.