Yiyan rọba silikoni olomi ti ara ẹni (LSR)

Ohun elo: imora pẹlu awọn sobusitireti ṣiṣu, gẹgẹbi, PC, PA, PET, PBT, PPSU, PEIetc.
Awọn ẹya ara ẹrọ bọtini: agbara giga, isunmọ to lagbara, vulcanization otutu kekere.
  • GA-2029X

  • Herchy

Wiwa:
Opoiye:

Idanwo: 130°C x 5min x 15MPa


Ọja sile
Ọja GA-2029X GA-2029X GA-2029X GA-2029X GA-2029X GA-2029X
Ifarahan Translucent

Igi (Pa.s)

A: 1000

B:2000

A:2000

B:3000

A:2000

B:4000

A:2000

B:4000

A:2000

B:4000

A: 5000

B: 6000
Lile ( ShoreA) 20 30 40 50
60
70
Ìwúwo (g/cm3) 5 7 8 8 8
7
Agbara fifẹ (MPa) 900
600
550
500
400
250
Ilọsiwaju(%) 10 10 15 25 25
30
Agbara omije (kN/m) 16 30 35
40 35
30










Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. Maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.