Selektiv o'z-o'zidan yopishqoq suyuq silikon kauchuk (LSR)

Ilova: PC, PA, PET, PBT, PPSU, PEI va boshqalar kabi plastik substratlar bilan bog'lash.
Asosiy xususiyatlar: yuqori quvvat, kuchli bog'lanish, past haroratli vulkanizatsiya.
  • GA-2029X

  • Herchi

Mavjudligi:
Miqdori:

Sinov: 130°C x 5min x 15MPa


Mahsulot parametrlari
Mahsulot GA-2029X GA-2029X GA-2029X GA-2029X GA-2029X GA-2029X
Tashqi ko'rinish Shaffof

Yopishqoqlik (Pa.s)

A: 1000

B: 2000

A: 2000

B: 3000

A: 2000

B: 4000

A: 2000

B: 4000

A: 2000

B: 4000

A: 5000

B: 6000
Qattiqlik (ShoreA) 20 30 40 50
60
70
Zichlik (g/sm3) 5 7 8 8 8
7
Kuchlanish kuchi (MPa) 900
600
550
500
400
250
Uzayish (%) 10 10 15 25 25
30
Yirilish kuchi (kN/m) 16 30 35
40 35
30










Oldingi: 
Keyingisi: 

TEZKOR havolalar

MAHSULOTLARIMIZ

BOG'LANISH UCHUN MA'LUMOT

Qo'shish: №33, 159-ko'cha, Taiye yo'li, Fengxian tumani, Shanxay
Tel / WhatsApp / Skype: +86 15221953351
Mualliflik huquqi     2023 Shanghai Herchy Rubber Co., Ltd. Sayt xaritasi |   Maxfiylik siyosati | Qo'llab-quvvatlash Leadong.