GA-2029X
Herchy
| Beschikbaarheid: | |
|---|---|
| Hoeveelheid: | |
Test: 130 °C x 5 min x 15 MPa
| Productparameters | |||||||
| Product | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | |
| Verschijning | Doorschijnend | ||||||
| Viscositeit (Pa.s) |
EEN: 1000 B: 2000 |
A:2000 B:3000 |
EEN:2000B :4000 |
EEN:2000B :4000 |
EEN:2000B :4000 |
EEN:5000 B:6000 |
|
| Hardheid (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Dichtheid (g/cm3) | 5 | 7 | 8 | 8 | 8 |
7 |
|
| Treksterkte (MPa) | 900 |
600 |
550 |
500 |
400 |
250 |
|
| Verlenging (%) | 10 | 10 | 15 | 25 | 25 |
30 |
|
| Scheursterkte (kN/m) | 16 | 30 | 35 |
40 | 35 |
30 |
|