Selective self-adhesive liquid silicone rubber (LSR)

Application: bonding with plastic substrates, such as, PC, PA, PET, PBT, PPSU, PEIetc.
Key features: high strength, strong bonding, low temperature vulcanization.
  • GA-2029X

  • Herchy

Availability:
Quantity:

Test: 130°C x 5min x 15MPa


Product parameters
ProductGA-2029XGA-2029XGA-2029XGA-2029XGA-2029XGA-2029X
AppearanceTranslucent

Viscosity(Pa.s)

A:1000

B:2000

A:2000

B:3000

A:2000

B:4000

A:2000

B:4000

A:2000

B:4000

A:5000

B:6000
Hardness (ShoreA)20304050
60
70
Density(g/cm3)57888
7
Tensile strength (MPa)900
600
550
500
400
250
Elongation(%)1010152525
30
Tear strength (kN/m)163035
4035
30










Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.