GA-91X3
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x5minx15MPa
| Product parameters | |||||
| Product | GA-9133 |
GA-9143 | GA-9153 | GA-9163 | GA-9173 |
| Appearance | Translucent | ||||
| Hardness (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Density(g/cm3) | 1.08 |
1.12 |
1.14 |
1.16 |
1.18 |
| Tensile strength (MPa) |
3.5 |
4.0 |
5.0 |
6.0 |
6.0 |
| Elongation(%) | 550 |
550 |
450 |
350 |
200 |
| Tear strength (kN/m) | 10 |
14 |
16 |
16 |
16 |
| Surface resistance (Ω) |
108--109 |
||||