GA-91X3
Herchy
| Argaeledd: | |
|---|---|
| Nifer: | |
Prawf: 1% o asiant halltu (50% past o DBPMH mewn gwm silicon), 175 ° x5minx15MPa
| Paramedrau cynnyrch | |||||
| Cynnyrch | GA-9133 |
GA-9143 | GA-9153 | GA-9163 | GA-9173 |
| Ymddangosiad | Tryleu | ||||
| Caledwch (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Dwysedd(g/cm3) | 1.08 |
1.12 |
1.14 |
1.16 |
1.18 |
| Cryfder tynnol (MPa) |
3.5 |
4.0 |
5.0 |
6.0 |
6.0 |
| elongation(%) | 550 |
550 |
450 |
350 |
200 |
| Cryfder dagrau (kN/m) | 10 |
14 |
16 |
16 |
16 |
| Gwrthiant arwyneb (Ω) |
108--109 |
||||