ꯖꯤ.ꯑꯦ.-꯹꯱ꯑꯦꯛꯁ꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫
ꯍꯔꯆꯤ꯫
| ꯐꯪꯒꯗꯕꯥ: | |
|---|---|
| ꯃꯁꯤꯡ: ꯱. | |
ꯇꯦꯁ꯭ꯠ: ꯀ꯭ꯌꯨꯔꯤꯡ ꯑꯦꯖꯦꯟꯇꯀꯤ 1% (ꯁꯤꯂꯤꯀꯣꯟ ꯒꯃꯗꯥ DBPMHꯒꯤ 50% ꯄꯦꯁ꯭ꯠ), 175° x5minx15MPa꯫
| ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫ | |||||
| ꯄꯣꯠꯊꯣꯛ | ꯖꯤ.ꯑꯦ.-꯹꯱꯳꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ |
ꯖꯤ.ꯑꯦ.-꯹꯱꯴꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯱꯵꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯱꯶꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯱꯷꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ |
| ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ | ꯇ꯭ꯔꯥꯟꯁꯂꯨꯁꯦꯟꯇ ꯑꯣꯏꯕꯥ꯫ | ||||
| ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. |
30 |
40 |
50 |
60 |
70 |
| ꯗꯦꯟꯁꯤꯇꯤ(ꯖꯤ/ꯁꯦ.ꯃꯤ.꯳) ꯑꯁꯤꯅꯤ꯫ | 1.08 |
1.12 |
1.14 |
1.16 |
1.18 |
| ꯇꯦꯟꯁꯥꯏꯜ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯃꯁꯨꯡ ꯑꯦꯝ.ꯄꯤ.ꯑꯦ. |
3.5 |
4.0 |
5.0 |
6.0 |
6.0 |
| ꯏꯂꯣꯡꯒꯦꯁꯟ(%) ꯴. | 550 |
550 |
450 |
350 |
200 |
| ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (kN/m) ꯑꯁꯤꯅꯤ꯫ | 10 |
14 |
16 |
16 |
16 |
| ꯁꯔꯐꯦꯁ ꯔꯦꯁꯤꯁ꯭ꯇꯦꯟꯁ (Ω) ꯑꯁꯤ . |
108--꯱꯰9 |
||||