GA-91X3 High grade antistatic silikoni rabala (mtundu wachilengedwe) (HCR)

Ntchito: gwiritsani ntchito kupanga antistatic roller, antistatic gasket, foni yam'manja, zidutswa za mafakitale.
Chofunikira chachikulu: zopanda pake, katundu wabwino kwambiri wa antistatic, perekani kutsimikizika kwa RoHS.
  • GA-91X3

  • Herchy

kupezeka:
kuchuluka:

Mayeso: 1% ya machiritso (50% phala la DBPMH mu chingamu cha silikoni), 175 ° x5minx15MPa

Zogulitsa katundu
Zogulitsa Mtengo wa GA-9133
Mtengo wa GA-9143 Mtengo wa GA-9153 GA-9163 GA-9173
Maonekedwe Zowoneka bwino
Kuuma (ShoreA)
30
40
50
60
70
Kachulukidwe (g/cm3) 1.08
1.12
1.14
1.16
1.18
Mphamvu yamagetsi (MPa)

3.5
4.0
5.0
6.0
6.0
Kutalikira (%) 550
550
450

350

200
Mphamvu yamisozi (kN/m) 10
14
16
16
16
Kukaniza pamwamba (Ω)
108--109









Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.