GA-91X3 Akwa ọkwa antistatic silicone roba (agba eke) (HCR)

Ngwa: tinye maka imepụta rola antistatic, gasket antistatic, ihe ndozi ekwentị mkpanaaka, iberibe ụlọ ọrụ dị iche iche.
Njirimara bụ isi: enweghị ụtọ, akụrụngwa antistatic mara mma, gafere nyocha nke RoHS.
  • GA-91X3

  • Herchy

Nnweta:
Ọnụọgụ:

Nnwale: 1% nke onye na-agwọ ọrịa (50% tapawa nke DBPMH na silicone gum), 175° x5minx15MPa

Ngwa ngwaahịa
Ngwaahịa GA-9133
GA-9143 GA-9153 GA-9163 GA-9173
Ọdịdị translucent
Isi ike (ShoreA)
30
40
50
60
70
Njupụta (g/cm3) 1.08
1.12
1.14
1.16
1.18
Ike tensile (MPa)

3.5
4.0
5.0
6.0
6.0
Mgbatị(%) 550
550
450

350

200
Ike akwa mmiri (kN/m) 10
14
16
16
16
Nguzogide elu (Ω)
108--109









Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.