GA-91X3
Herchy
| Beschikbaarheid: | |
|---|---|
| Aantal: | |
Test: 1% verharder (50% DBPMH-pasta in siliconengom), 175° x5minx15MPa
| Productparameters | |||||
| Product | GA-9133 |
GA-9143 | GA-9153 | GA-9163 | GA-9173 |
| Verschijning | Doorschijnend | ||||
| Hardheid (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Dichtheid (g/cm3) | 1.08 |
1.12 |
1.14 |
1.16 |
1.18 |
| Treksterkte (MPa) |
3.5 |
4.0 |
5.0 |
6.0 |
6.0 |
| Verlenging (%) | 550 |
550 |
450 |
350 |
200 |
| Scheursterkte (kN/m) | 10 |
14 |
16 |
16 |
16 |
| Oppervlakteweerstand (Ω) |
108--109 |
||||