GA-91X3 Silicone rɔba a ɛyɛ den a ɛko tia (abɔde mu kɔla) (HCR) .

Dwumadi: fa di dwuma ma wɔyɛ antistatic roller, antistatic gasket, mobile phone fixture,miscellaneous asinasin a mfiridwuma.
Key feature: tasteless, antistatic agyapade a eye kyɛn so, twam nokwaredi a RoHS.
  • GA-91X3 na ɛwɔ hɔ

  • Herchy a ɔyɛ ɔbarima

Nea Ɛwɔ Hɔ:
Dodow:

Sɔhwɛ: 1% a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175° x5minx15MPa

Nneɛma a wɔyɛ no parameters
Adwadeɛ GA-9133 na ɛwɔ hɔ
GA-9143 na ɛwɔ hɔ GA-9153 na ɛwɔ hɔ GA-9163 na ɛwɔ hɔ GA-9173 na ɛwɔ hɔ
Mmaeɛ Ɛyɛ nea ɛyɛ translucent
Nneɛma a ɛyɛ den (ShoreA) .
30
40
50
60
70
Nsuo a ɛyɛ den(g/cm3) . 1.08
1.12
1.14
1.16
1.18
Ahoɔden a wɔde twe ade (MPa) .

3.5
4.0
5.0
6.0
6.0
Ntrɛwmu(%) . 550
550
450

350

200
Ahoɔden a ɛtetew mu (kN/m) . 10
14
16
16
16
Nneɛma a ɛko tia asase ani (Ω) .
108--109









Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.