GA-32×0J
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1.3% of curing agent (50% paste of DCBP in silicone gum),130°C x 5min x 15MPa
| Product parameters | |||||
| Product | GA-3240J | GA-3250J | GA-3260J | GA-3270J | GA-3280J |
| Appearance | Transparent | ||||
| Williamplasticity | 180 | 210 | 260 | 280 | 310 |
| Hardness (ShoreA) | 42 | 52 | 58 | 68 | 78 |
| Density(g/cm3) | 1.11 | 1.14 | 1.17 | 1.20 | 1.22 |
| Tensile strength (MPa) | 9 | 10 | 9 | 9 | 8 |
| Elongation(%) | 600 | 550 | 450 | 350 | 250 |
| Tear strength (kN/m) | 18 | 22 | 22 | 22 | 22 |