GA-32×0J
Herchy
| Boteng: | |
|---|---|
| Bongata: | |
Teko: 1.3% ea moemeli oa phekolo (50% peista ea DCBP ka silicone gum), 130 ° C x 5min x 15MPa
| Lihlahisoa tsa lihlahisoa | |||||
| Sehlahisoa | GA-3240J |
GA-3250J | GA-3260J | GA-3270J | GA-3280J |
| Ponahalo | Tse pepeneneng | ||||
| Williamplasticity |
180 |
210 |
260 |
280 |
310 |
| Ho thatafala (LebopoA) |
42 |
52 |
58 |
68 |
78 |
| Boima ba 'mele(g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Tensile Matla (MPa) |
9 |
10 |
9 |
9 |
8 |
| Elongation(%) | 600 |
550 |
450 |
350 |
250 |
| Matla a ho lla (kN/m) | 18 |
22 |
22 |
22 |
22 |