Toets: 1,3% verhardingsmiddel (50% pasta van DCBP in silikoongom), 130°C x 5min x 15MPa
| Produk parameters | |||||
| Produk | GA-3240J |
GA-3250J | GA-3260J | GA-3270J | GA-3280J |
| Voorkoms | Deursigtig | ||||
| Williamplastisiteit |
180 |
210 |
260 |
280 |
310 |
| Hardheid (ShoreA) |
42 |
52 |
58 |
68 |
78 |
| Digtheid (g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Treksterkte (MPa) |
9 |
10 |
9 |
9 |
8 |
| Verlenging (%) | 600 |
550 |
450 |
350 |
250 |
| Skeursterkte (kN/m) | 18 |
22 |
22 |
22 |
22 |