Tel: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
Prodakt dɛn .
Yu de ya: Os » Prodakt dɛn . » Sintesis rɔba . » VMQ silikon na di . » GA-32×0J Jɛnɛral pɔpɔshɔn silikon rɔba fɔ ɛkstrushɔn (fumed silika) (HCR)

Loading na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na na .

Share to:
Fɛsbuk sherin bɔtin .
Twitter sherin bɔtin .
Layn sherin bɔtin .
WeChat sherin button .
LinkedIn Sharing bɔtin .
Pinterest Sharing bɔtin .
WhatsApp Sharing bɔtin .
ShareThis Sharing bɔtin .

GA-32×0J Jɛnɛral pɔpɔshɔn silikon rɔba fɔ ɛkstrushɔn (fumed silika) (HCR)

Aplikeshɔn: fayn fɔ di prodakshɔn fɔ gas faz ɛkstrushɔn prodak lɛk hos,siling strip ɛn ɔda tin dɛn.
Ki ficha: gud anti-yellowing prɔpati, fayn fayn prɔsesab小ty,pas diɔthɛntishɔn fɔ RoHS, REACH, ɛn LFGB.
  • GA-32 × 0J we de na di wɔl

  • Herchy na di .

Di tin dɛn we yu kin gɛt:
Kwantiti: .

Tεst: 1.3% pan di kכring ejen (50% paste fכ DCBP insay silikon gכm),130°C x 5min x 15MPa


Prodakt Paramita dɛn .
Sɔntin GA-3240J we de na di wɔl
GA-3250J we dɛn kɔl GA-3260J we de na di wɔl GA-3270J we dɛn kɔl GA-3280J we dɛn kɔl
Aw a luk Klia
WiliamPlastisiti .
180
210
260
280
310
Hadnɛs (Shorea) .
42
52
58
68
78
Densiti(g/cm3) . 1.11
1.14
1.17
1.20
1.22
Tensil Strɔng (MPA) .

9
10
9
9
8
Elongeshɔn(%) . 600
550
450
350
250
Strɔng fɔ wata (KN/M) . 18
22
22
22
22








Bifo: 
Nɛks: 

Kwik Links .

Wi Prodakt dɛn .

Kɔntakt infɔmeshɔn .

Add: No.33, Lane 159, Taiye Rod, Fengxian Distrikt, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kopirayt     2023 Shanghai Herchy Rubber Co., Ltd. Saytmap . |   Prayvesi Polisi | Sɔpɔt bay . Leadong.