Ikizamini: 1,3% yumuti ukiza (50% paste ya DCBP mumashanyarazi ya silicone), 130 ° C x 5min x 15MPa
| Ibipimo byibicuruzwa | |||||
| Ibicuruzwa | GA-3240J |
GA-3250J | GA-3260J | GA-3270J | GA-3280J |
| Kugaragara | Mucyo | ||||
| Yamamoto |
180 |
210 |
260 |
280 |
310 |
| Gukomera (ShoreA) |
42 |
52 |
58 |
68 |
78 |
| Ubucucike (g / cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Imbaraga zingana (MPa) |
9 |
10 |
9 |
9 |
8 |
| Kurambura (%) | 600 |
550 |
450 |
350 |
250 |
| Amarira amarira (kN / m) | 18 |
22 |
22 |
22 |
22 |