GA-32×0J hmanga siam a ni
Herchy a ni
| A awm theihna: | |
|---|---|
| A zat: | |
Test: Curing agent 1.3% (silicone gum-a DCBP paste 50%),130°C x 5min x 15MPa
| Product Parameters 1000 a ni. | |||||
| Thilsiam | GA-3240J a ni |
GA-3250J hmanga siam a ni | GA-3260J a ni | GA-3270J hmanga siam a ni | GA-3280J hmanga siam a ni |
| Landan | Langtlang | ||||
| Williamplasticity . |
180 |
210 |
260 |
280 |
310 |
| Harsatna (Shorea) . |
42 |
52 |
58 |
68 |
78 |
| Density(g/cm3) a ni. | 1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Tensile chakna (MPA) . |
9 |
10 |
9 |
9 |
8 |
| A sei zawng(%) . | 600 |
550 |
450 |
350 |
250 |
| Tear chakna (kn/m) . | 18 |
22 |
22 |
22 |
22 |