GA-32 × 0 J
Herchy
| Muaj: | |
|---|---|
| Quantity: | |
Kev Ntsuas: 1.3% ntawm tus neeg sawv cev kho (50% muab tshuaj txhuam DCBP hauv cov pos hniav silicone), 130 ° C x 5min x 15MPa
| Khoom parameters | |||||
| Khoom | GA-3240J |
GA-3250J | GA-3260J | GA-3270J | GA-3280J |
| Qhov tshwm sim | Pob tshab | ||||
| Williamplasticity |
180 |
210 |
260 |
280 |
310 |
| Hardness (ShoreA) |
42 |
52 |
58 |
68 |
78 |
| Qhov ceev (g / cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Tensile zog (MPa) |
9 |
10 |
9 |
9 |
8 |
| Elongation (%) | 600 |
550 |
450 |
350 |
250 |
| Lub zog tawg (kN / m) | 18 |
22 |
22 |
22 |
22 |