GA-32×0J
Herchy
| Helitaanka: | |
|---|---|
| Tirada: | |
Tijaabada: 1.3% wakiilka daawaynta (50% koollada DCBP ee xanjada silikoonka), 130°C x 5min x 15MPa
| Xuduudaha alaabta | |||||
| Alaabta | GA-3240J |
GA-3250J | GA-3260J | GA-3270J | GA-3280J |
| Muuqashada | Hufan | ||||
| Williamplasticity |
180 |
210 |
260 |
280 |
310 |
| Adag ( ShoreA) |
42 |
52 |
58 |
68 |
78 |
| Cufnaanta (g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.22 |
| Xoog xajin (MPa) |
9 |
10 |
9 |
9 |
8 |
| Dheeraynta(%) | 600 |
550 |
450 |
350 |
250 |
| Xoogga jeexjeexa (kN/m) | 18 |
22 |
22 |
22 |
22 |