GA-2040 LSR mo nga taputapu Taura (LSR)

Whakaahuatanga hua:kotahi momo rapa silicone wai ngaohiko-atete teitei o nga waahanga e rua na te matatini konukawata, ko te tauwehenga A/B ko te 1:1, ko te waahanga A me te B 1 he maamaa me te hina, he ahua.
Te tono: nga taputapu taura ngaohiko takawaenga, te kapeka whakaheke makariri o roto, o waho hoki, te hononga whakawhiti, te pukoro. 
Ko nga waahanga matua: te werohanga werohanga, te kaha teitei, te roanga teitei, te kaha o te roimata, te riipene whakatika iti, te tere whakaora tere, te whakamana i te RoHS me te REACH.
  • GA-2040

  • Herchy

Wātea:
Rahi:

Whakamātautau: 130°C x 10min, 200°C x 4H.

Tawhā hua

Hua GA-2040-35T
GA-2040-35
GA-2050-35 GA-2040-45
Te ahua Puatarangi Kerei Whero Kerei
Maama (ShoreA) 35-42 35-42 48 42
Kiato(g/cm 3) 1.13
1.13
1.14
1.12
Te kaha o te kaha (MPa) 9.5
9.5 9.0
9.5
Whakaroa(%) 800 800 650 800
Te kaha roimata (kN/m) 40 40 35
40
Tau wera wera 153°C±3°C×7D Hurihia te kaha tensile%) <土10 <土10 <土10 <土10
Te huringa o te whakaroa
<土10 <土10 <土10 <土10
He rereke tonu i te toronga tonu 300% x 90°C x 168H
<5% <5% <5% <5%
Dielectric tamau i 100HZ 3.03 3.03 3.03 2 95
Tauwehe tohanga i100HZ 0.0029 0.0029 0.0029 0.0029
Te ātete ki te rerenga hiko me te tohu 1A3.5 1A3.5 1A3.5 1A4.5
Kaha Dielectric (kV/mm) 24
24
22
23
Rōrahi Ātete (Ω·cm) 1.0 *1015 1.0 *1015 1.0 *1015 1.0 *1015




Tōmua: 
Panuku: 

NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.