GA-2040 LSR rau Cable Accessories (LSR)

Cov lus piav qhia: ib yam ntawm high-voltage-resistant kua silicone roj hmab ntawm ob feem catalyzed los ntawm platinum complex, lub A / B piv li 1: 1, tivthaiv A thiab B 1s pob tshab thiab grey, feem.
Daim ntawv thov: intermediate voltage cable accessories, sab hauv thiab sab nraud txias shrink davhlau ya nyob twg, kev hloov kev sib koom tes, sheath. 
Cov yam ntxwv tseem ceeb: txhaj tshuaj molding, siab tensile, siab elongation, siab tsim kua muag lub zog, me me kho tensionset, ceev curing ceev, dhau qhov authentication ntawm RoHS thiab REACH.
  • TSI-2040

  • Herchy

Muaj:
Quantity:

Ntsuas: 130 ° C x 10min, 200 ° C x 4H.

Khoom parameters

Khoom GA-2040-35T
UA-2040-35
UA-2050-35 UA-2040-45
Qhov tshwm sim Translucent Grey Liab Grey
Hardness (ShoreA) 35-42 : kuv 35-42 : kuv 48 42
Qhov ceev (g / cm3 3) 1.13
1.13
1.14
1.12
Tensile zog (MPa) 9.5
9.5 9.0
9.5
Elongation (%) 800 800 650 800
Lub zog tawg (kN / m) 40 40 35
40
Lub hnub nyoog kub tsis kam 153 ° C ± 3 ° C × 7D Hloov lub zog tensile (%) < 10 < 10 < 10 < 10
Hloov ntawm elongation
< 10 < 10 < 10 < 10
Permanent deformation ntawm qhov txuas ntxiv 300% x 90 ° C x 168H
<5% <5% <5% <5%
Dielectric qhov tsis tu ncua ntawm 100HZ 3.03 3.03 3.03 2 95
Dissipation factor ntawm 100HZ 0.0029 0.0029 0.0029 0.0029
Kev tiv thaiv hluav taws xob thiab kev kos npe 1 A3.5 1 A3.5 1 A3.5 1a4.5 ua
Dielectric zog (kV / mm) 24
24
22
23
VolumeResistivity (Ω·cm) 1.0 * 1015 1.0 * 1015 1.0 * 1015 1.0 * 1015




Yav dhau los: 
Tom ntej: 

QUICK LINKS

Peb cov khoom

Tiv tauj xov xwm

Ntxiv: No.33, Txoj Kev 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Daim duab qhia chaw |   Txoj Cai Tswjfwm Ntiag Tug | Txhawb nqa By Leadong.