GA-2040 LSR ma Nhama a Wɔde Yɛ Nhama (LSR) .

Product description:ɔkwan biako a ɛkorɔn voltage-resistant nsu silicone rɔba a abien componentcatalyzed denam platinum complex, A / B ratio sɛ ​​1 :1, ade A ne B 1s transparent ne grey,sɛnea ɛte biara.
Application: mfinimfini voltage cable accessories, emu ne akyi awɔw shrink terminal,nsakrae nkwaa,sheath. 
Nneɛma atitiriw:injection molding, tensile a ɛkorɔn, elongation a ɛkorɔn, ahoɔden a ɛkorɔn tear,ketewa fix tensionset, ntɛmntɛm curing ahoɔhare, twa nokwaredi a RoHS ne REACH.
  • GA-2040 na ɛwɔ hɔ

  • Herchy a ɔyɛ ɔbarima

Nea Ɛwɔ Hɔ:
Dodow:

Sɔhwɛ: 130°C x simma 10, 200°C x 4H.

Nneɛma a wɔyɛ no parameters

Adwadeɛ GA-2040-35T na ɛwɔ hɔ
GA-2040-35 na ɛwɔ hɔ
GA-2050-35 na ɛwɔ hɔ GA-2040-45 na ɛwɔ hɔ
Mmaeɛ Ɛyɛ nea ɛyɛ translucent Nso Kɔkɔɔ Nso
Nneɛma a ɛyɛ den (ShoreA) . 35-42 na ɛwɔ hɔ 35-42 na ɛwɔ hɔ 48 42
Nsuo a ɛyɛ den(g/cm 3) . 1.13
1.13
1.14
1.12
Ahoɔden a wɔde twe ade (MPa) . 9.5
9.5 9.0
9.5
Ntrɛwmu(%) . 800 800 650 800
Ahoɔden a ɛtetew mu (kN/m) . 40 40 35
40
Mfe a wɔadi a ɛyɛ hyew a wɔko tia 153°C±3°C×7D Nsakrae a ɛba wɔ tensile ahoɔden mu(1) . <土10 na ɛwɔ hɔ <土10 na ɛwɔ hɔ <土10 na ɛwɔ hɔ <土10 na ɛwɔ hɔ
Nsakrae a ɛba wɔ elongation mu
<土10 na ɛwɔ hɔ <土10 na ɛwɔ hɔ <土10 na ɛwɔ hɔ <土10 na ɛwɔ hɔ
Daa deformation wɔ daa ntrɛwmu 300% x 90°C x 168H
<5% . <5% . <5% . <5% .
Dielectric daa wɔ 100HZ 3.03 3.03 3.03 2 95
Nneɛma a ɛtrɛw wɔ100HZ 0.0029 0.0029 0.0029 0.0029
Ɛko tia anyinam ahoɔden a ɛretu ne agyiraehyɛde 1A3.5 1A3.5 1A3.5 1A4.5
DielectricAhoɔden (kV/mm) . 24
24
22
23
Nnyigyei a Ɛko Tia (Ω·cm) . 1.0 *10 na ɛwɔ hɔ15 1.0 *10 na ɛwɔ hɔ15 1.0 *10 na ɛwɔ hɔ15 1.0 *10 na ɛwɔ hɔ15




Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.