GA-2040
Herchi
| Mavjudligi: | |
|---|---|
| Miqdori: | |
Sinov: 130°C x 10min, 200°C x 4H.
| Mahsulot parametrlari | |||||
| Mahsulot | GA-2040-35T |
GA-2040-35 |
GA-2050-35 | GA-2040-45 | |
| Tashqi ko'rinish | Shaffof | Kulrang | Qizil | Kulrang | |
| Qattiqlik (ShoreA) | 35-42 | 35-42 | 48 | 42 | |
| Zichlik (g/sm 3) | 1.13 |
1.13 |
1.14 |
1.12 |
|
| Kuchlanish kuchi (MPa) | 9.5 |
9.5 | 9.0 |
9.5 |
|
| Uzayish (%) | 800 | 800 | 650 | 800 | |
| Yirilish kuchi (kN/m) | 40 | 40 | 35 |
40 |
|
| Issiq yoshga qarshilik 153 ° C ± 3 ° C × 7D | Kuchlanish kuchining o'zgarishi (% )) | <10 | <10 | <10 | <10 |
| Uzayishning o'zgarishi |
<10 | <10 | <10 | <10 | |
| Doimiy kengaytmada doimiy deformatsiya 300% x 90 ° C x 168H |
<5% | <5% | <5% | <5% | |
| 100 Gts da dielektrik doimiy | 3.03 | 3.03 | 3.03 | 2 95 | |
| 100 Gts da tarqalish koeffitsienti | 0.0029 | 0.0029 | 0.0029 | 0.0029 | |
| Elektr qochqinning qarshiligi va markalash | 1A3.5 | 1A3.5 | 1A3.5 | 1A4.5 | |
| Dielektrik quvvat (kV/mm) | 24 |
24 |
22 |
23 | |