GA-2040
Herchy
| kupezeka: | |
|---|---|
| kuchuluka: | |
Mayeso: 130 ° C x 10min, 200 ° C x 4H.
| Zogulitsa katundu | |||||
| Zogulitsa | Mtengo wa GA-2040-35T |
GA-2040-35 |
GA-2050-35 | GA-2040-45 | |
| Maonekedwe | Zowoneka bwino | Imvi | Chofiira | Imvi | |
| Kuuma (ShoreA) | 35-42 | 35-42 | 48 | 42 | |
| Kachulukidwe (g/cm 3) | 1.13 |
1.13 |
1.14 |
1.12 |
|
| Mphamvu yamagetsi (MPa) | 9.5 |
9.5 | 9.0 |
9.5 |
|
| Kutalikira (%) | 800 | 800 | 650 | 800 | |
| Mphamvu yamisozi (kN/m) | 40 | 40 | 35 |
40 |
|
| Kukana zaka kutentha 153 ° C± 3 ° C× 7D | Kusintha kwamphamvu kwamphamvu (((()) | <土10 | <土10 | <土10 | <土10 |
| Kusintha kwa kutalika |
<土10 | <土10 | <土10 | <土10 | |
| Kupindika kosatha pakukulitsa kosalekeza 300% x 90°C x 168H |
<5% | <5% | <5% | <5% | |
| Dielectric nthawi zonse pa 100HZ | 3.03 | 3.03 | 3.03 | 2 95 | |
| Dissipation factor pa 100HZ | 0.0029 | 0.0029 | 0.0029 | 0.0029 | |
| Kukaniza kutayikira kwamagetsi ndikuyika chizindikiro | 1A3.5 | 1A3.5 | 1A3.5 | 1A4.5 | |
| Mphamvu ya Dielectric (kV/mm) | 24 |
24 |
22 |
23 | |
| VolumeResistivity (Ω·cm) | 1.0 * 1015 | 1.0 * 1015 | 1.0 * 1015 | 1.0 * 1015 | |