GA-2040 LSR kubikoresho bya Cable (LSR)

Ibisobanuro byibicuruzwa: ubwoko bumwe bwumuvuduko mwinshi wihanganira amazi ya silicone reberi yibice bibiri byasesenguwe na platine, igipimo cya A / B nka 1: 1, igice A na B 1s kibonerana kandi gifite imvi.
Gushyira mu bikorwa: ibikoresho bya interineti hagati ya voltage ibikoresho, imbere no hanze bikonje bikonje bigabanuka, inzibacyuho ihuriweho, sheath. 
Ibyingenzi byingenzi: gushushanya inshinge, kurakara cyane, kuramba cyane, imbaraga zamarira nyinshi, gukosora bito bito, gukira byihuse, kunyura ibyemezo bya RoHS na REACH.
  • GA-2040

  • Herchy

Kuboneka:
Umubare:

Ikizamini: 130 ° C x 10min, 200 ° C x 4H.

Ibipimo byibicuruzwa

Ibicuruzwa GA-2040-35T
GA-2040-35
GA-2050-35 GA-2040-45
Kugaragara Birasobanutse Icyatsi Umutuku Icyatsi
Gukomera (ShoreA) 35-42 35-42 48 42
Ubucucike (g / cm 3) 1.13
1.13
1.14
1.12
Imbaraga zingana (MPa) 9.5
9.5 9.0
9.5
Kurambura (%) 800 800 650 800
Amarira amarira (kN / m) 40 40 35
40
Imyaka ishyushye 153 ° C ± 3 ° C × 7D Guhindura imbaraga zingana (%) <土 10 <土 10 <土 10 <土 10
Guhindura kuramba
<土 10 <土 10 <土 10 <土 10
Guhindura burundu kwaguka guhoraho 300% x 90 ° C x 168H
<5% <5% <5% <5%
Dielectric ihoraho kuri 100HZ 3.03 3.03 3.03 2 95
Ikintu cyo gutandukana kuri 100HZ 0.0029 0.0029 0.0029 0.0029
Kurwanya kumeneka kw'amashanyarazi no gushiraho ikimenyetso 1A3.5 1A3.5 1A3.5 1A4.5
Imbaraga za Dielectric (kV / mm) 24
24
22
23
Umubyigano (Ω · cm) 1.0 * 1015 1.0 * 1015 1.0 * 1015 1.0 * 1015




Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.