Telefon: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
NUSIWO WOWƆ
Èle afisia: Aƒeme » Nusiwo Wowɔ » Nuwɔwɔ ƒe Rubber » VMQ Silicone ƒe dɔwɔwɔ » GA-2040 LSR na kaƒomɔ̃wo (LSR)

agbatsɔtsɔ

Mamã na:
facebook dzi mamã ƒe dzesi
twitter dzi mamã ƒe dzesi
fliwo mama ƒe dzesi
wechat mama ƒe dzesi
linkedin ƒe mama ƒe dzesi
pinterest mama ƒe dzesi
whatsapp mamã ƒe dzesi
sharethis mamã ƒe dzesi

GA-2040 LSR na ka ƒe kpeɖeŋutɔ (LSR) .

Adzɔnu ƒe numeɖeɖe:ɖeka ƒomevi gã-tsitretsitsi tsi silicone rababa ƒe eve componentcatalyzed to platinum complex, le A / B ratio abe 1 :1, akpa A kple B 1s transparent kple grey,respectively.
Dɔwɔwɔ: domedome voltage ka kpeɖeŋutɔ, ememe kple egodo vuvɔ shrink terminal,trɔtrɔ ƒunukpeƒe,sheath. 
Vevietɔ nɔnɔmewo:injection molding, kɔkɔ tensile, kɔkɔ elongation, kɔkɔ aɖatsi ŋusẽ,sue ɖɔ tensionset, kabakaba dɔyɔyɔ duƒuƒu, to nyateƒetoto RoHS kple REACH.
  • GA-2040 ƒe agbalẽ

  • Herchy ƒe ame

Nusiwo Li:
Agbɔsɔsɔ:

Dodokpɔ: 130°C x 10min, 200°C x 4H.

Nusiwo wowɔ ƒe nɔnɔmewo

Nu si wowɔ GA-2040-35T ƒe agbalẽa
GA-2040-35 ƒe agbalẽ
GA-2050-35 ƒe agbalẽ GA-2040-45 ƒe agbalẽ
Dzedzeme Nusi me kɔ nyuie Fu Dzẽ Fu
Sesẽme (ƑutaA) . 35-42 me 35-42 me 48 42
Eƒe kpekpeme(g/cm 3) . 1.13
1.13
1.14
1.12
Ŋusẽ si wotsɔna ƒoa nu (MPa) . 9.5
9.5 9.0
9.5
Elongation(%) ƒe didime . 800 800 650 800
Aɖatsi ƒe ŋusẽ (kN/m) . 40 40 35
40
Ƒe ƒe dzoxɔxɔ ƒe tsitretsitsi 153°C±3°C×7D Tɔtrɔ le tensile ŋusẽ ŋu(1) . <土10 <土10 <土10 <土10
Trɔtrɔ le didime ŋu
<土10 <土10 <土10 <土10
Deformation mavɔ le kekeɖenudɔ madzudzɔmadzudzɔe 300% x 90°C x 168H
<5% . <5% . <5% . <5% .
Dielectric ɣesiaɣi le 100HZ 3.03 3.03 3.03 2 95
Nusiwo kakana le 100HZ 0.0029 0.0029 0.0029 0.0029
Tsitretsitsi ɖe elektrikŋusẽ ƒe sisi kple dzesidede ŋu 1A3.5 1A3.5 1A3.5 1A4.5
Dielektrikŋusẽ ƒe Ŋusẽ (kV/mm) . 24
24
22
23
Agbɔsɔsɔme ƒe Tsitretsitsi (Ω·cm) . 1.0 *1015 1.0 *1015 1.0 *1015 1.0 *1015




Si do ŋgᴐ: 
Esi kplᴐe ɖo: 

Adzɔnuwo ƒe Kafukafu si Do Ƒome Kplii

NYAWO ƑE ƑOMEDODO KABA

MÍAƑE NUWO ƑE NUWO

NYATAKAKA SIWO WOÐO BE WOAÐO BE WOAÐE KPƆKPƆ

Tsɔ kpe ɖe eŋu: No.33, Mɔdodo 159, Taiye Mɔ dzi, Fengxian Nutome, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nutata ƒe Gomenɔamesi     2023 Shanghai Herchy Rubber Co., Ltd. Nyatakakadzraɖoƒe ƒe Nɔnɔmetata |   Ameŋunyatakakawo Ŋuti Ðoɖo | Kpekpeɖeŋu To Leadong ƒe agbalẽ.