Test: 1.3% of curing agent (50% paste of DCBP in silicone gum),130°C x 5min x 15MPa.
| Product parameters | |||||
| Product | GA-3331 | GA-3341 | GA-3351 | GA-3361 | GA-3371 |
| Appearance | Translucent | ||||
| Williamplasticity | 150 | 215 | 260 | 280 | 310 |
| Hardness (ShoreA) | 42 | 52 | 60 | 70 | 78 |
| Density(g/cm3) | 1.13 | 1.18 | 1.19 | 1.22 | 1.22 |
| Tensile strength (MPa) | 7.5 | 7.5 | 7.5 | 7 | 7 |
| Elongation(%) | 550 | 450 | 350 | 250 | 200 |