GA-10×3J Pa'u silicone fa'amoemoe lautele mo le fa'aosoina (HCR)

Fa'aoga: mea fa'apipi'i masani e pei ole uaea, uaea, fa'agaau, fa'apipi'i ma isi.
Fa'ailoga autu: vave fa'aosoina, lelei le fa'atinoina o le eletise, fa'agaioiga lelei, pasi le fa'amaoni o le RoHS, REACH, ma le FDA
  • GA-10×3J

  • Herchy

Avanoa:
Aofa'i:

Suʻega: 1.3% o le vailaʻau faʻamalolo (50% paʻu o le DCBP i le silicone gum), 130 ° C x 5min x 15MPa.


Fa'atauga o oloa
Oloa GA-3331
GA-3341 GA-3351 GA-3361 GA-3371
Fa'aaliga Translucent
Williamplasticity
150
215
260
280
310
Malosi (ShoreA)
42
52
60
70
78
Malosi (g/cm3) 1.13
1.18
1.19
1.22
1.22
Malosi fa'amalosi (MPa)

7.5
7.5
7.5
7
7
Fa'atele(%) 550
450
350
250
200
Malosi o loimata (kN/m) 16
20
20
20
16








Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AMATALAGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.