GA-10×3J ƒe ƒuƒoƒo
Herchy ƒe ame
| : | |
|---|---|
| Agbɔsɔsɔ: | |
Dodokpɔ: 1.3% le atike si daa gbe le ame ŋu (50% ƒe atike si wotsɔ DCBP wɔe le silicone gum me),130°C x 5min x 15MPa.
| Nusiwo wowɔ ƒe nɔnɔmewo | |||||
| Nu si wowɔ | GA-3331 ƒe agbalẽa |
GA-3341 ƒe agbalẽa | GA-3351 ƒe agbalẽa | GA-3361 ƒe agbalẽa | GA-3371 ƒe agbalẽa |
| Dzedzeme | Nusi me kɔ nyuie | ||||
| Williamplasticity ƒe dɔwɔwɔ |
150 |
215 |
260 |
280 |
310 |
| Sesẽme (ƑutaA) . |
42 |
52 |
60 |
70 |
78 |
| Eƒe kpekpeme(g/cm3) . | 1.13 |
1.18 |
1.19 |
1.22 |
1.22 |
| Ŋusẽ si wotsɔna ƒoa nu (MPa) . |
7.5 |
7.5 |
7.5 |
7 |
7 |
| Elongation(%) ƒe didime . | 550 |
450 |
350 |
250 |
200 |
| Aɖatsi ƒe ŋusẽ (kN/m) . | 16 |
20 |
20 |
20 |
16 |