GA-10×3J
Herchy
| Ketersediaan: | |
|---|---|
| Kuantitas: | |
Pengujian: 1,3% bahan pengawet (50% pasta DCBP dalam permen karet silikon),130°C x 5 menit x 15MPa.
| Parameter produk | |||||
| Produk | GA-3331 |
GA-3341 | GA-3351 | GA-3361 | GA-3371 |
| Penampilan | Tembus cahaya | ||||
| Williamplastisitas |
150 |
215 |
260 |
280 |
310 |
| Kekerasan (ShoreA) |
42 |
52 |
60 |
70 |
78 |
| Massa jenis (g/cm3) | 1.13 |
1.18 |
1.19 |
1.22 |
1.22 |
| Kekuatan tarik (MPa) |
7.5 |
7.5 |
7.5 |
7 |
7 |
| Pemanjangan(%) | 550 |
450 |
350 |
250 |
200 |
| Kekuatan sobek (kN/m) | 16 |
20 |
20 |
20 |
16 |