GA-10 × 3J
Herchy
| Kuboneka: | |
|---|---|
| Umubare: | |
Ikizamini: 1,3% yumuti ukiza (50% paste ya DCBP mumashanyarazi ya silicone), 130 ° C x 5min x 15MPa.
| Ibipimo byibicuruzwa | |||||
| Ibicuruzwa | GA-3331 |
GA-3341 | GA-3351 | GA-3361 | GA-3371 |
| Kugaragara | Birasobanutse | ||||
| Yamamoto |
150 |
215 |
260 |
280 |
310 |
| Gukomera (ShoreA) |
42 |
52 |
60 |
70 |
78 |
| Ubucucike (g / cm3) | 1.13 |
1.18 |
1.19 |
1.22 |
1.22 |
| Imbaraga zingana (MPa) |
7.5 |
7.5 |
7.5 |
7 |
7 |
| Kurambura (%) | 550 |
450 |
350 |
250 |
200 |
| Amarira amarira (kN / m) | 16 |
20 |
20 |
20 |
16 |