GA-10×3J
Herchy
| Ho fumaneha: | |
|---|---|
| Bongata: | |
Teko: 1.3% ea moemeli oa phekolo (50% pente ea DCBP ka silicone gum), 130 ° C x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | |||||
| Sehlahisoa | GA-3331 |
GA-3341 | GA-3351 | GA-3361 | GA-3371 |
| Ponahalo | Translucent | ||||
| Williamplasticity |
150 |
215 |
260 |
280 |
310 |
| Ho thatafala (LebopoA) |
42 |
52 |
60 |
70 |
78 |
| Boima ba 'mele(g/cm3) | 1.13 |
1.18 |
1.19 |
1.22 |
1.22 |
| Tensile Matla (MPa) |
7.5 |
7.5 |
7.5 |
7 |
7 |
| Elongation(%) | 550 |
450 |
350 |
250 |
200 |
| Matla a ho lla (kN/m) | 16 |
20 |
20 |
20 |
16 |