Sɔhwɛ: 1.3% a ɛyɛ aduru a ɛsa yareɛ (50% a wɔde ahyɛ DCBP mu wɔ silicone gum mu),130°C x 5min x 15MPa.
| Nneɛma a wɔyɛ no parameters | |||||
| Adwadeɛ | GA-3331 na ɛwɔ hɔ |
GA-3341 na ɛwɔ hɔ | GA-3351 na ɛwɔ hɔ | GA-3361 na ɛwɔ hɔ | GA-3371 na ɛwɔ hɔ |
| Mmaeɛ | Ɛyɛ nea ɛyɛ translucent | ||||
| Williamplasticity a wɔde yɛ nneɛma |
150 |
215 |
260 |
280 |
310 |
| Nneɛma a ɛyɛ den (ShoreA) . |
42 |
52 |
60 |
70 |
78 |
| Nsuo a ɛyɛ den(g/cm3) . | 1.13 |
1.18 |
1.19 |
1.22 |
1.22 |
| Ahoɔden a wɔde twe ade (MPa) . |
7.5 |
7.5 |
7.5 |
7 |
7 |
| Ntrɛwmu(%) . | 550 |
450 |
350 |
250 |
200 |
| Ahoɔden a ɛtetew mu (kN/m) . | 16 |
20 |
20 |
20 |
16 |