GA-10×3J Xikongomelo xo angarhela xa rhaba ya silicone yo humesa (HCR) .

Ku tirhisiwa: switirhisiwa swa ntolovelo swa extrusion swofana na o邸narywire, cable, hose, gluestrip etc.
Swihlawulekisi swa nkoka: rivilo ra extrusion hi ku hatlisa, matirhelo ya kahle ya gezi, processab川ty ya kahle swinene,ku hundza ku tiyisisiwa ka RoHS, REACH, na FDA
  • GA-10×3J ya xirhendzevutani

  • Herchy

Ku kumeka:
Nhlayo:

Xikambelo: 1.3% wa xiaki xo horisa (50% wa paste ya DCBP eka silicone gum),130°C x 5min x 15MPa.


Tipharamitha ta swikumiwa
Ximakiwa GA-3331
GA-3341 GA-3351 GA-3361 GA-3371
Xivumbeko Ku vonakala loku vonakaka
Williamplasticity ya vumaki
150
215
260
280
310
Ku nonoka (ShoreA) .
42
52
60
70
78
Ku tsindziyela(g/cm3) . 1.13
1.18
1.19
1.22
1.22
Ku tiya ka ku tsana (MPa) .

7.5
7.5
7.5
7
7
Ku leha(%) . 550
450
350
250
200
Matimba ya ku handzuka (kN/m) . 16
20
20
20
16








Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.