Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x 5min x 15MPa.
| Product parameters | ||||||
| Product | GA-9035A/B |
GA-9041A/B | GA-9051A/B | GA-9061A/B | GA-9071A/B | GA-9081A/B |
| Appearance | Transparent | |||||
| Williamplasticity |
150 |
190 |
210 |
240 |
270 |
290 |
| Hardness (ShoreA) |
36 |
40 |
50 |
60 |
70 |
80 |
| Density(g/cm3) | 1.10 |
1.13 |
1.16 |
1.18 |
1.19 |
1.21 |
| Tensile strength (MPa) |
10 |
9.0 |
10.0 |
10.0 |
9.5 |
9.0 |
| Elongation(%) | 1050 |
900 |
700 |
600 |
500 |
400 |
| Tear strength (kN/m) | 25 |
30 |
35 |
35 |
35 |
35 |
| Rebound(%) |
60 |
55 |
55 |
50 |
50 |
|