GA-9035A / B Platinum yatangije reberi ya silicone yo kuvura (HCR)

Gusaba: bikwiranye no gukora ibicuruzwa byubuvuzi.
Ibyingenzi byingenzi: imbaraga nyinshi, gukorera mu mucyo, umutungo mwiza wo kurwanya umuhondo, udafite uburozi kandi utaryoshye, unyuze kuri RoHS, REACH, FDA, LFGB. Kora ikizamini cya 1S010993 biocompatib 山 ty.
  • GA-9035A / B.

  • Herchy

Kuboneka:
Umubare:

Ikizamini: 1% yumuti ukiza (50% paste ya DBPMH mumase ya silicone), 175 ° x 5min x 15MPa.


Ibipimo byibicuruzwa
Ibicuruzwa GA-9035A / B.
GA-9041A / B. GA-9051A / B. GA-9061A / B. GA-9071A / B. GA-9081A / B.
Kugaragara Mucyo
Yamamoto
150
190
210
240
270
290
Gukomera (ShoreA)
36
40
50
60
70
80
Ubucucike (g / cm3) 1.10
1.13
1.16
1.18
1.19
1.21
Imbaraga zingana (MPa)

10
9.0
10.0
10.0
9.5
9.0
Kurambura (%) 1050
900
700
600
500
400
Amarira amarira (kN / m) 25
30
35
35
35
35
Kwisubiraho (%)
60
55
55
50
50








Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.