GA-9035A/B
Herchy
| Boteng: | |
|---|---|
| Bongata: | |
Teko: 1% ea moemeli oa phekolo (50% peista ea DBPMH ka silicone gum), 175 ° x 5min x 15MPa.
| Lihlahisoa tsa lihlahisoa | ||||||
| Sehlahisoa | GA-9035A/B |
GA-9041A/B | GA-9051A/B | GA-9061A/B | GA-9071A/B | GA-9081A/B |
| Ponahalo | Tse pepeneneng | |||||
| Williamplasticity |
150 |
190 |
210 |
240 |
270 |
290 |
| Ho thatafala (LebopoA) |
36 |
40 |
50 |
60 |
70 |
80 |
| Boima ba 'mele(g/cm3) | 1.10 |
1.13 |
1.16 |
1.18 |
1.19 |
1.21 |
| Tensile Matla (MPa) |
10 |
9.0 |
10.0 |
10.0 |
9.5 |
9.0 |
| Elongation(%) | 1050 |
900 |
700 |
600 |
500 |
400 |
| Matla a ho lla (kN/m) | 25 |
30 |
35 |
35 |
35 |
35 |
| Rebound(%) |
60 |
55 |
55 |
50 |
50 |
|