GA-9035A/B Platinum catalyzed silicone rubber ya vutshunguri (HCR) .

Xitirhisiwa: xi lulamerile ku humelerisa switirhisiwa swa vutshunguri.
Swihlawulekisi swa nkoka: matimba ya le henhla, ku vonakala lokukulu, nhundzu ya kahle yo lwisana na ku tshwuka,a yi na chefu na ku pfumala nantswo, hundza eka ku tiyisisiwa ka RoHS, REACH, FDA, LFGB.Pass the test of 1S010993 biocompatib山ty.
  • GA-9035A/B

  • Herchy

Ku kumeka:
Nhlayo: .

Xikambelo: 1% wa xiaki xo horisa (50% wa paste ya DBPMH eka silicone gum), 175° x 5min x 15MPa.


Tipharamitha ta Xiendliwa .
Ximakiwa GA-9035A/B
GA-9041A/B GA-9051A/B GA-9061A/B GA-9071A/B GA-9081A/B
Xivumbeko Erivaleni
WilliamPlasticity .
150
190
210
240
270
290
Ku nonoka (ShoreA) .
36
40
50
60
70
80
Ku tsindziyela(g/cm3) . 1.10
1.13
1.16
1.18
1.19
1.21
Ku tiya ka ku koka (MPa) .

10
9.0
10.0
10.0
9.5
9.0
Ku leha(%) . 1050
900
700
600
500
400
Matimba ya ku handzuka (kN/m) . 25
30
35
35
35
35
Ku tlhelela endzhaku(%) .
60
55
55
50
50








Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.